An alumina HTCC green tape is chosen for the fired part it must produce, not for a single headline number · Shrinkage, purity, the conductor paste and the firing profile all interact
The values below are typical laboratory figures from HTK grade specification sheets · Use them to shortlist, then confirm them on your own line
1 Start from the fired dimension
Shrinkage decides how green dimensions translate into fired dimensions · Laboratory values are a starting point; lamination pressure, temperature and the firing profile shift them, so re-measure under your own conditions before freezing artwork
* HTKAHP100 values are reference figures at 100 μm sheet thickness and 34.3 MPa press pressure
| Grade | XY (%) | Z (%) |
|---|---|---|
| HTK96 | 13.6±0.5 | 28 |
| HTKAHP100 | 13.0–14.0 * | 19–23 * |
| HTKA9996 | 15.1 | 23 |
| HTKAHP200 | 16 | 20 |
2 Choose purity by what the part must do
Higher alumina content generally brings lower dielectric loss and higher strength, but it is not automatically the right choice · HTKAHP100 has the highest thermal conductivity of the four grades (36 W/m·K) and the lowest firing range (1430–1530 °C)
| Grade | Al₂O₃ | Thermal conductivity (W/m·K) | Flexural strength (MPa) | Dielectric loss @ 1 MHz |
|---|---|---|---|---|
| HTK96 | 96% | ≥18 | ≥350 | ≤0.001 |
| HTKAHP100 | >97% | 36 | >380 | <0.4×10⁻⁴ |
| HTKA9996 | ≥99.6% | ≥28 | ≥400 | ≤2.5×10⁻⁴ |
| HTKAHP200 | ≥99.98% | ≥28 | ≥400 | ≤2.5×10⁻⁴ |
3 Evaluate tape and conductor as one system
HTCC is co-fired with refractory-metal conductors · HTK supplies three tungsten pastes — via filling (HTK-4T), via wall coating (HTK-1G) and screen printing (HTK-2Y) — co-fired at 1520–1560 °C in H₂/N₂ and qualified with HTKA9996 and HTKAHP200 · HTK96 co-fires with W and Mo · Check that the paste firing window overlaps the tape firing window before planning a build
4 Check the process window
Lamination, binder burnout and co-firing profiles differ by grade · Use the grade sheet as the starting profile and adjust it on your furnace
| Grade | Peak firing | Notes |
|---|---|---|
| HTK96 | 1520–1560 °C, 2 h | Lamination 85 °C, 30 MPa, 30 min; burnout 1 °C/min to 600 °C, 3 h |
| HTKAHP100 | 1430–1530 °C, 1 h | Lamination 80–110 °C, 14.7–34.3 MPa; burnout ≤2 °C/min to 500 °C, 5 h |
| HTKA9996 | 1500–1550 °C, 3 h | |
| HTKAHP200 | 1450–1550 °C, 3 h |
5 What to ask for in a sample lot
- Grade, or the property that matters most
- Sheet size and green thickness
- Quantity — trial lots start from 100 sheets
- Matched paste: via fill, via wall coating or printing